In brief

A dry table can suit uniform, prepared feed when a dry output matters. Wet separation is worth testing when feed varies, fine copper is lost to plastic, or a second recovery stage is needed. Compare both with the same material, and account for the whole process.

1. How the separation methods work

Both methods separate copper or aluminium from polymer insulation after the cable is shredded. A dry density table blows air through a vibrating, inclined deck. Dense particles tend to stay in contact with the deck and travel toward the concentrate outlet, while the airflow fluidises the lighter fraction. Dust extraction is normally part of the dry process.

Wet separation uses water as the separating medium. On a wet shaking table, flowing water and deck motion move particles along different paths. Density matters, but particle size and shape also affect settling and transport. Not all plastics float: PVC can be denser than water.

Density of metals, polymers and water (g/cm³)

  • Polyethylene0.92
  • Water1
  • PVC1.4
  • Aluminium2.7
  • Copper8.96

Typical reference values; polymer density varies by formulation.

2. Sorting the feed

Mixed wire sizes are harder to separate consistently on an air table. Fine strands can report to the plastic fraction when they are processed alongside larger pieces. Sorting by conductor size or classifying the granulate helps, but adds equipment, handling and stock between stages.

A wet route can reduce the need to pre-sort mixed cable. A representative sample is still needed: liberated particles, intact cable fragments and tangled strands do not behave the same way.

3. Particle size and grinding

The Russian analysis contrasts fine preparation, around 3–5 mm for the dry route discussed, with a coarser route for selected thick-conductor feeds. Finer grinding can improve liberation but increases energy use, knife and screen wear, and dust.

For a wet process, the analysis discusses elongated fragments in the 10–50 mm range from selected feeds. Screen aperture and final particle length are not interchangeable: a long, narrow piece can pass through a smaller opening. The right screen and feed preparation depend on the cable construction and the separation test.

4. Fine wire and mixed feedstocks

Telephone cable, twisted pair, computer wiring and automotive harnesses can produce very fine or tangled copper. A dry line may use a turbo mill, air classifier or zigzag separator to improve liberation and narrow the size distribution.

A wet table is worth testing on mixed fines and on plastic tailings that still contain copper. It cannot recover copper that has not been liberated from insulation, and recovery must be measured rather than inferred from the appearance of the concentrate.

5. Concentrate purity and metal recovery

Purity and recovery are different. Purity tells you how much of the concentrate is the target metal. Recovery tells you how much of the metal in the feed reached that concentrate. To compare processes, measure both and check the metal remaining in the tailings.

Moisture, oil, gel and adhesive can make particles stick together, particularly in dry separation. Water can help in some cases, but troublesome feedstocks should be tested for both separation performance and water handling.

6. Limits and advantages of dry tables

Dry separation avoids a process water circuit and does not require a downstream dryer. For a clean, uniform, well-prepared feed, this can outweigh the extra grinding and classification.

Dust collection, sensitivity to damp material and loss of fines can make mixed feed more difficult. The Russian analysis flags sub-0.5 mm copper as particularly challenging in its dry scenario; that is not a universal cut-off. Throughput depends on the equipment and feed, not just on whether separation is wet or dry.

7. Cleaning aluminium granulate

Wet density separation can be tested as a finishing step to remove heavier copper or lead particles from aluminium granulate. Aluminium is about 2.70 g/cm³ and copper about 8.96 g/cm³, so a density-based route can be an alternative to an optical sorter if the materials are sufficiently liberated.

A cleaner fraction can command a better price. The Russian version discusses an illustrative 25% price difference; actual prices depend on grade, the buyer and the market. UMT's SM 24.6 wet separator can be evaluated for these duties using samples.

8. What copper losses cost

At an assumed copper value of RUB 1,000,000 per tonne, a 1% loss costs RUB 10,000 per tonne of contained copper. These are scenario figures, not commodity quotes or performance guarantees.

For a tonne of cable containing 30% copper by weight, the same 1% loss is 3 kg of copper, or RUB 3,000 at that assumed price.

Copper losses: cost per tonne of contained copper (RUB thousands)

  • 1%10
  • 2%20
  • 5%50
  • 10%100
  • 12%120

Illustrative calculation at RUB 1,000,000 per tonne of copper.

9. Wet vs dry at a glance

Air separation

  • No process water or drying.
  • Fits well-prepared, relatively uniform dry feed.
  • May need extra grinding, sizing and dust extraction.
  • Test fine copper losses and polymer carryover.

Water separation

  • Can handle selected mixed and coarser feeds and reprocess tailings.
  • Can upgrade aluminium granulate by removing denser particles.
  • Allow for water circulation, treatment or disposal as needed, dewatering and drying.
  • Confirm wear, wet-metal storage and protection from freezing.

10. When to choose each process

Start with a dry-table trial if the feed is already sorted and granular, process water is limited, or the product must come off the line dry. Include the cost of dust extraction and any additional preparation.

Trial wet separation for mixed cable, selected armoured or gel-filled feeds, copper-aluminium radiator scrap and plastic tailings. Compare the whole process, including water, drying, throughput and the sale value of both output fractions.

11. Practical recommendation

Test both processes using representative samples if the choice is not clear. Weigh the feed, concentrate and tailings, sample each for metal content, and report purity, recovery and throughput separately. Then compare the value of recovered metal against the cost of preparation, separation and any drying.

The Russian edition discusses dry losses of 5–12% and wet losses below 1% for its comparison. Use these as scenarios, not guaranteed results for a machine or feedstock.

All cable recycling articles